Dry Bags Recalled over Loose Magnets: How Should Adhesive Joints and Small-Magnet Risks Be Included in Procurement Acceptance Checks?
Fidlock Hermetic dry bags have been recalled because adhesive strips at the closure can detach and magnets can fall out. This article explains how buyers can assess adhesive durability, magnet retention and small-part risks.

Why a small adhesive strip can become a serious risk
On November 19, 2026, the CPSC recalled approximately 490 Fidlock Hermetic dry bags. The adhesive strip in the closure area can detach, allowing the magnets inside to fall out. If swallowed, high-powered magnets can attract one another and cause intestinal injuries.
Procurement takeaway: Buyers need to assess waterproof performance, adhesive service life and the harm that could result from detached magnets together.
Common causes of adhesive joint failure
Temperature, humidity, sweat, cleaning agents and ultraviolet light can all affect the adhesive layer. The surface energies of the materials also affect bonding. If a factory performs only a short tensile test at room temperature, the result cannot represent long-term use.
Suggested verification methods
Environmental aging
Buyers can request high- and low-temperature cycling, damp heat, sweat exposure and cleaning-agent exposure tests. Peel strength and closure performance should be checked again after aging.
Magnet retention
Magnets should have independent mechanical restraints and should not rely on a layer of adhesive alone. Testing should cover pulling, bending, dropping and repeated opening and closing.
Failure modes
Teams should distinguish between adhesive peeling, substrate rupture and exposed magnets in their records. If any failure can release small magnets, the risk rating needs to be increased.
Evidence buyers can request
| Evidence | Purpose |
|---|---|
| Adhesive specifications and shelf life | Prevent use of expired or incorrect adhesive |
| Surface preparation records | Confirm preparation before bonding |
| Test data after aging | Verify long-term performance |
| Magnet batch records | Support traceability and recalls |
Scope and limitations
This article does not replace regulatory testing for small parts and magnets. Products that children may come into contact with need a stricter assessment.
FAQ
Can using more adhesive solve the problem?
Not necessarily. An excessively thick adhesive layer can also suffer cohesive failure. Engineering teams should first confirm the materials, surface preparation and curing conditions.
Is passing a waterproof test enough?
No. Waterproof testing focuses on liquid ingress, while magnet retention testing focuses on parts coming loose. The two tests serve different purposes.
Is mechanical fastening mandatory?
Regulations do not necessarily impose a uniform requirement, but mechanical restraints can reduce the risks associated with failure of an adhesive joint alone.
Recommended actions for procurement teams
Buyers should retest bond strength after aging and confirm that magnets will not detach because of a single-point failure.
Suggested use on stellar.shop
The platform can record suppliers' bonding processes, environmental testing capabilities and experience in managing magnetic components.
References
- U.S. CPSC, Fidlock GmbH Recalls Hermetic Dry Bags, 2026-11-19: https://www.cpsc.gov/Recalls/2027/Fidlock-GmbH-Recalls-Hermetic-Dry-Bags-Due-to-Risk-of-Serious-Injury-or-Death-from-Magnet-Ingestion-Hazard